MAISHI WIRE MESH MANUFACTURE GROUP is a professional stainless steel wire mesh manufacturer since 1986, now we will talk about the main mesh defects.
1. General mesh defects
The general mesh defects of paper making stainless steel mesh mainly refers to the slight unevenness of the mesh surface, slight rolling, spotted oil stains, small sundries, mild wavy edges, single broken wires, nest wefts, noses, small loose lines, small jumps line, wrong twist, etc. The number of common mesh defects is 10 square meters and cannot exceed 5.
2. Major mesh defects
The main defects of paper making stainless steel mesh refers to:
1) forks, holes (more than 3 broken menstruation);
2) uneven mesh surface;
3) half cut weft (length greater than 50mm);
4) thin secret road;
5) Lightly wound;
6) Lightly inclined;
7) Partially wrinkled, creased, corrugated;
8) Large jumper (length greater than 10mm);
9) Larger loose, double, and parallel (length greater than 30mm) , lotus leaf edge or wavy edge.
3. Serious mesh defects
The major defects of paper making stainless steel mesh refers to:
(1) The warp and weft are not firmly intertwined, and the two fingers are used to move up and down, and the warp and weft yarns have obvious loose displacement phenomenon;
(2) The net slope is severe, and the width of the web width of the warp and weft is not more than 4 degrees;
(3) hole, half latitude, and large fork;
(4) The extra large mesh holes in the radial direction exceed the tolerance;
(5) The warp and weft diameters are seriously out of tolerance;
(6) A large number of creases;
(7) Large area density is out of tolerance;
(8) Large-area running latitude, the mesh surface is uneven;
(9) The serious color difference of large area is uneven and the mechanical damage is serious.
If you have any need for stainless steel mesh, welcome to contact MAISHI WIRE MESH MANUFACTURE GROUP.